CLASSIFICATIONS: E91T-GM per AWS A5.29

This all position, low alloy, flux cored electrode is designed to weld low alloy steels where a minimum tensile strength of 90,000 psi is required.

APPLICATIONS: When good low temperature toughness and a minimum tensile strength of 90,000 psi are needed, Select 937Ni represents an outstanding choice. Lack of fusion is not a problem due to this wire’s deep penetrating characteristics. Typical applications include offshore structures, earthmoving machinery and other specialized structural uses requiring good low temperature toughness.

DIAMETERS:
.045", .052", 1/16"

SHIELDING GAS: 75-80% Ar/20-25% CO2, 40-55 cfh

WELDING POSITIONS: All positions

CHARACTERISTICS:

  • Good arc drive.
  • Very positive, smooth and stable arc transfer with low spatter emission.
  • Fast freezing slag is easily removed.

    TYPICAL MECHANICAL PROPERTIES
      75% Ar/
    25% CO2
    Ultimate Tensile Strength (psi) 99,600
    Yield Strength (psi) 87,000
    Percent Elongation 23
    CVN (ftlb f) @ -20° F 80
    CVN (ftlb f) @ -40° F 70
    CVN (ftlb f) @ -60° F 55

    TYPICAL DEPOSIT COMPOSITION
    Wt% C Mn P S Si Ni
    75 Ar/25 CO2
    .07 1.60 .008 .008 .20 2.60

    RECOMMENDED WELDING PARAMETERS*
      Optimum Range
    Diam. Position Amps Volts WFS Amps Volts
    1/16" Flat 350 28 350 150-400 22-33
      Overhead 225 25 180 150-310 22-28
      Vertical up 225 24 180 150-280 22-27
    .052" Flat 300 27 440 100-330 19-31
      Overhead 200 25 245 150-310 21-28
      Vertical up 200 24 245 150-280 21-27
    .045" Flat 250 27 450 100-300 21-31
      Overhead 190 25 305 150-280 21-29
      Vertical up 190 24 305 100-230 21-28

  •